In MTC , if Weld metal , Mn > 1.6 % , then A NO can not  be A NO - 1 
Pl; check and do needful accordingly

You can do the following - 
Hope what A no you mentioned above , have been qualified  with PQR brands , both SAW Wire and Flux.
Make A no as   ----
Address Brand names of PQR 'S SAW Wire and SAW flux in PQR and WPS both.
Ensure that CMTR is EN 10204 TYP 3.1 

Thanks 
Vishwas - IWE 
InternationaL Welding Engineer 
Head - Welding Technology 



On Mon, Nov 14, 2022 at 8:50 AM williams p wilson <williamswilsonp@gmail.com> wrote:
Dear Experts,

As per Sec.IX. Table QW-442 (A Numbers) for A-No.1, Mn (Max %) is 1.60 , but one of our Kiswel SAW MTC is having 1.63 (wt. %) Mn in the chemical composition of the weld metal under PWHT Condition (602 Deg.C x 9 Hrs) - It can be considered under A No.1 - Please confirm

Thank You & Regards
Williams P Wilson
+968-94600828
QA/QC Engineer
Please consider the environment before printing this message

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHBxnQ40m1NOWXEgi-%2BYWy7wzAe1UY7ND%3DhiegCtsf6%3DDc2DMA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3O-Sp6pFPhn5csw0Yg75PAu8dGb%3D1%3D9hSOPJd8_pJ%2BuXA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...