Thursday, September 29, 2022

[MW:33514] Impact Test Requirement : ASME Sec. VIII Div.1

Dear Experts, 

Please share the Impact Test requirements of SA 516 Gr.70 N , 80 mm thickness with a MDMT of -29 degree C.

Thank You & Regards
Williams P Wilson
+968-94600828
QA/QC Engineer
Please consider the environment before printing this message

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHBxnQ7-ZGwD2T5SHytyTQndeSpueg2kxmG%3DJg5S6cKHMspPUg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...