Re: [MW:33297] Pickling and passivation need before painting SS surfaces

Pickling and passivation is  Not required  ,   because you are going for painting after completion of NDE but  for the process side (Accessible Root) you may need to perform if purging is not maintained properly. or any heat tints found unacceptable.
 
If you  painting is not involved ,  Yes, it is required to perform the  pickling and passivation of SS weldments 100% as due to heat generation  during welding the passivation layer will be damaged and may not be formed naturally, in general  Passivation will form naturally in air & it may take longer time to form for protection to occur. Before this period, passivation by using Chemicals may be carried out rapidly. as we are not checking for confirmation of the passivation layer formation. 

 refer any client specifications Ex. DEP 30.10.60.18 / ADNOC specifications about this requirements for stainless steels  welds 

Regards,
Srinuvasa Rao

On Tue, Jul 26, 2022 at 12:35 PM sajeed zaheer <sajeed7674@gmail.com> wrote:
ASTM A 380

On Tue, Jul 26, 2022 at 11:19 AM Anilkumar G <akg.nitt@gmail.com> wrote:
Dear Experts

Do we need pickling and passivation of SS surfaces before painting them? Could you please suggest any specification relevant this requirement?
The parts are SS cast valves requiring painting.

Regards
Anilkumar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/754e0d61-54e1-420e-ae4b-f92593266f5en%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFycdMz9RbXVXteXk%2B3MvOj%3D%2B2ftw-bu-N9jAx1tsvtrz3L7Gw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHdRSONAmRhoaZnSZgQjndMMsC4WZ085EyncChWJXO3fDGdBiA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...