Re: [MW:33292] 3.2 requirement

EN10204   3.2 certification is Specific testing of each HEAT under the supervision and testing of Manufacture Representative at Pipe mill involving various stages of testing as accepted with Manufacturer representative.

If 3.2 is the requirement then the service has to be considered Critical and normally without MTC I would scrap it.

If 1 or 2 testing has been omitted then you can discuss with the Client for witness at the Accredited LAb.

Discuss with your Client.

Thanks & Regards

J.Gerald Jayakumar




On Tuesday, 26 July, 2022 at 08:58:15 am GMT+4, mithlesh kumar <mithleshmech47@gmail.com> wrote:


Dear Expert,

we have some pipes of 316 material all pipes are off cut and heat identification is not available on these pipes. MTC type requirement is 3.2 also we have not MTC. what is the Procedure to certify the material as per the 3.2 type requirement? 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c083e4ed-c02a-49dc-b2a4-c3d8c8c8c738n%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...