Kindly help me to clarify and explain the impact test requirements for procedure qualification (PQR)

 Qus #1: P15E material (p91 A335) ferrtic alloy steel need to qualify is it required impact test ?  How to check reference code B31.3 impact requirements table please explain

Qus# 2: regarding for PWHT requirements for mentioned material if it is impact test means PWHT range comes under essential so if PWHT 740 deg celuis doing PQR . Then WPS also same temperature required to perform PWHT? But b31.3 mentioned some ranges ex 700-800 deg celuis. I have doubt this ranges normally if essential variable means we need follow the value rather than range so PWHT how to I perform the PQR did temperature or b31.3 mentioned temperature ranges?

Please advise 

Thanks and regards
Kannan Ponnikumar
QC Inspector

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKL%3DdYwfvUoBWUjzexz6hxU0G8Euwbwdo%3DCV1sD5LfAz2-O-JQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...