Re: [MW:33086] Filler wire selection

625+304H it is better to NiCr3 or NiCr Fe2

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Fri, May 20, 2022 at 8:46 AM 'Karthik' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Hi,
1. Inconel 625 to SS 304H : ENiCrFe-2 or ENiCrMo-3
2. Inconel 625 to SS316L : ENiCrFe-2 or ENiCrMo-3


Thanks& Regards,

(Karthik)
Karthikeyan.S
M: +66-892512282


On Monday, May 16, 2022, 12:05:37 PM GMT+7, chandra sekaran <chandrasekaran.vcs@gmail.com> wrote:


Dear experts kindly guide me For GTAW 

1. Inconel 625 to SS 304H : what filler wire can be use 

2. Inconel 625 to SS316L : 
What filler wire can be use

Regards

Chandrasekaran V

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4ibzmvO7S7PhStVFoVfO%3D97tuRBY_f3_ak9Nz_hACR%3DEeTCw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/645978729.351719.1653013969725%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNwn8sjBfS2KDs9HhrRt5%3DfAbnLZ--vbLdf2jBSkHHOnA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...