Re: [MW:32986] Super duplex PQR for corrosion test.

Pls also add Test temperature

Thanks & Regards

J.Gerald Jayakumar



On Monday, 21 March, 2022, 07:50:54 am GMT+4, 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:


Please provide details like

Grade
Type of corrosion test like ASTM G48 method A
Shielding and purging gas
corrosion test failure due to weight loss or pitting
Welding consumable
Oxygen purity maintained in the purge gas

Thanks & Regards

J.Gerald Jayakumar




On Monday, 21 March, 2022, 07:21:40 am GMT+4, PK M <pkmqaqc@gmail.com> wrote:


Dear Experts,

 

We have recently failed the super duplex PQR for corrosion test.


So please suggest how to successfully super duplex PQR with a corrosion test.


Any prevention for corrosion test or all other tests for Super Duplex stainless steel.


Thank you.

Pk

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFoQ_ncfpaPnA3GzgcTGCFywhxihTUZ5z42j5NDAmbRJM2dzCg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/134282676.572393.1647834598145%40mail.yahoo.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...