Yes you could refer to VIII-1

Στις Τετ, 23 Φεβ 2022, 06:00 ο χρήστης 'Sankaran Sp' via Materials & Welding <materials-welding@googlegroups.com> έγραψε:
Dear friends,

We used to get A217 - WC6 & A217 -WC9 casting from foundry with  normalising & tempering conditions, these details are given the MTC of the product. while checking the soaking hours for normalising & tempering process, they used to follow 4 hours for all 100 to 200 thickness jobs, when as asked to maintain 5 hours for 125mm, 6 hours for 150mm & 8 hours for 200mm thickness, they refused to increase the soaking hours from 4 hours and asking the reference standard for soaking hours, in this situation shall we refer ASME sec VIII div-1 for soaking hours w.r.to P nos? kindly help me in this regards.      .    


Regards,
Sankaran.SP
Coimbatore, India. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2118283400.531862.1645459089014%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40DgrEAEOuyrCMrHFck3qFpdRaMxAj6KDcSCjCY7vNiG9w%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...