Re: [MW:32819] Re: Impact test ASME b 31.3 ed. 2020

if ur requirement for HAZ also, then u have to test again, otherwise no

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Mon, Feb 7, 2022 at 2:48 PM Mohd Siraj <mohd52100@gmail.com> wrote:
just adding,

for PQR qualification, impact test cant be exempted if require by service, there are many discussions in the forum, 
by providing MTC of consumable, " YOUR CONSUMABLE JUST ELIGIBLE TO WELD OR USE" for said applicable.

based on consumable MTC or base metal MTC, you cant just get a waiver in PQR.

purpose of PQR to check all combinations of base metal+ consubamble+welder+machine are able to produce the desired results.

On Friday, December 10, 2021 at 6:21:21 AM UTC+3 ROLANDO RC wrote:
Good afternoon, My name is Rolando and I just registered. The forum is excellent!

I bring the following doubt about the table Table 323.2.2 Requirements for low temperature toughness tests for metals ASME B31.3 2020

As we can see, it has a revision in table A-3 (b) (2020) where I understand that if I have a certified welding consumable with impact test I can exempt said test in the WPS qualification, for example:

If I have a SA-333 gr 6 material with manufacturing certificate and charpy according to the standard (18 J to -45), it can be welded with a consumable E 7018-1 certified by the factory with charpy (27 J to -45)
If I use this combination on my PQR, can I waive the impact test on my PQR weld? ... assuming I already have a metal base and a factory crash tested consumables certificate? (then I interpret table 323.2.2 table A-3 does not speak of the ZAC)

greetings and thanks!

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f2ac85bf-8652-4b6e-83b2-6eb6d9c70d94n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNTfS2QbeqoDgxjAAbk14iBrKNXTjk7-1kf-OK8HUJvEQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...