Tuesday, February 8, 2022

[MW:32826] Re: REQUIRED FILLER WIRE FOR (ASTM A312-Gr UNS 31254) Super Austenetic Stainless Steel

Avesta P54 is a good choice for SAS and it is affluently available in KSA, very cost effective.
just take care of good cleaning and avoid any kind of moisture on the surface and hope u pass G48!

On Tuesday, February 8, 2022 at 6:18:00 AM UTC+3 Muhammad Azeem wrote:
Gents,
I need your valuable support to assist about the filler wire to be used for Super Austenitic Stainless Steel (ASTM A 312 Gr UNS 31254) ??




Regards,

Muhammad Azeem Iqbal
Welding Inspector Aramco Approved
053110-8577/0554453626/0590071467


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8e1f3a9f-2d27-44fa-b777-6a9e6ed119ddn%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...