Monday, February 7, 2022

[MW:32817] Re: GRP Information

for GRP, use only manufacture tolence,

who is your supplier?  CPI or else.

mfg is providing dia and thk tolenrece bassed their process to make this pipe, fitting , t connection, as you know all are made from grp filament have difference tolerance mfg to mfg.

for other qualification work also u can request their procedure or MOS.



On Sunday, December 26, 2021 at 7:46:57 PM UTC+3 Ahmed Rashed wrote:

Dear all,

Hope to be in a good health

I need to know how can i make material receiving for GRP piping and fitting 

Like which standard to check the dimension of piping and fitting ( ovality , length , thickness ..etc)

Thanks in advance

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e238d8f6-2099-49fa-8ced-757ce0e9755bn%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...