Re: [MW:32782] Corrosion Resistant Overlay over Carbon steel Preheat Requirements

what is Carbon steel thickness?

On Mon, 24 Jan 2022, 15:06 Vinoth kanna ramachandran, <srvkanna1@gmail.com> wrote:
Dear Welding Experts,

Preheat to be maintained or not for overlay of filler metal E309L-17 over carbon steel.
Any ASME clause referring to that, is highly appreciated.


Regards

Vinoth kanna
Gulf petrochemical Services I Oman

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADbO-YaO7gu01ayUO%2BceJoidxUNW_PTKyUM3VES-x_VSmc3U2w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3MaL77m5CW7VLimvmQ_1iMiv8gqiWWsi1M%3DcMQxYFMGOg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...