Tuesday, January 18, 2022

Re: [MW:32762] Weld overlay vs Explosion bonding for monel

Dear Dev :
pl make it more clear   SS 304L + Monel

On Tue, 11 Jan 2022 at 11:36, Devalkumar Desai <dd101189@gmail.com> wrote:
Dear all, 

Plese advice better option for
Tubesheet:  SS 304L + Monel. 

1) Weld overlay . (Is possible??) 
2) Explosion Bonded. 

Br, 
Deval

On Mon, 10 Jan, 2022, 08:47 'dwh' via Materials & Welding, <materials-welding@googlegroups.com> wrote:

Has the component been case -hardened?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2236ce4c.b5800.17e3ef143ac.Webtop.103%40btinternet.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM94n3pDAgAFZLqm5F9AWxO8SyGtdHaS_kE0kJ36tf%3DQNdWhpQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BQ29Ojzm-EYCM9LQ%3D-d52AHyh6OwokoMJDHwE2Yc_uTpVH59Q%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...