Re: [MW:32634] Re: Hydrotest as per ASME B 31.3

Dear All,
Yes...The leak test means  Hytrotest also.
Regards,
SOLOMAN PETER
TTSJV Project
Bahrain

On Tue, Nov 30, 2021 at 6:14 AM Sagar SK <sagar.kadam@rencons.com> wrote:

345.3 Preparation for Leak Test
345.3.1 Joints Exposed
(d) All joints may be primed and painted prior to leak
testing unless a sensitive leak test (para. 345.8) is
required.

Regards,

On Tuesday, 12 October 2021 at 14:47:49 UTC+3 kkmec...@gmail.com wrote:
Dear Experts,
As per b 31.3 Joints can be painted before leak test. Is the leak test referred here as a hydrotest also? Please confirm.


Best Regards,

 

Krishna Kamal Nayan  


 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7397a251-fc13-4417-9cc3-40e623f58458n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMvP5sy7rL%2Bt7p0VdeBq73s4fnpyPeD%2BGvHxJJX5H5mWZHx0hg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...