Thursday, November 25, 2021

Re: [MW:32618] Digest for materials-welding@googlegroups.com - 4 updates in 1 topic

Reply to the question of Mr K D Pandithan

As per the recommendation of Special Metals--US A
 Following grades are recommended for dissimilar welding of 625 to grade 310 S Steel



1--INCONEL 617==ERNICRCOMO-1       FOR HIGHEST TEMP SERVICE (INCO 617 HAS HIGH COBALT CONTENT)

2--INCONEL 625==ERNICRMO-3       FOR MEDIUM TEMP  SERVICE 

3--INCONEL 82=ERNICR-3               FOR LOWER SERVICE TEMP  
 

Regards

C  C GIROTRA
=====================================================================================


On Thu, Nov 25, 2021 at 10:23 AM <materials-welding@googlegroups.com> wrote:
Kannayeram Gnanapandithan <kgpandithan@gmail.com>: Nov 24 10:59AM +0530

inconel 625
 
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE, CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer.
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349
 
 
Arun Padman <arunpadman0105@gmail.com>: Nov 24 10:23AM +0300

Dear,
 
ER NiCrMo-3 is suitable to weld 625 to 600/625/825/C-22/B-2 etc., not 310.
 
Regards,
 
*Arun Padman Manayil*
P Save a tree. Please don't print this e-mail unless you really need to
 
 
Kannayeram Gnanapandithan <kgpandithan@gmail.com>: Nov 24 02:45PM +0530

Why Inconel 625 is not suitable, could you elaborate to understand.
 
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE, CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer.
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349
 
 
On Wed, Nov 24, 2021 at 1:39 PM Arun Padman <arunpadman0105@gmail.com>
wrote:
 
sajeed zaheer <sajeed7674@gmail.com>: Nov 24 12:18PM +0300

For the first point the filler you can used ER Ni cr Mo-3
For dish head after cold forming it depends on fiber elongation of
material usually 5 to 10 fiber elongation PWHT is required and above 10
Normalizing and tempering is required.
 
You received this digest because you're subscribed to updates for this group. You can change your settings on the group membership page.
To unsubscribe from this group and stop receiving emails from it send an email to materials-welding+unsubscribe@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMrhEo-HvnxeGXvFwHZnfvhcHTTr89U51o82ViDxz4j5_bxBGQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...