Wednesday, June 23, 2021

Re: [MW:32427] PREHEAT TEMPERATURE

Dear Manoj,
               Please also refer as mentioned in ASME SEC IX for your query.............
QW-406.3 PREHEAT An increase of more than 55Deg C in the maximum interpass temperature recorded on the PQR. This variable does not apply when a WPS is qualified with a PWHT above the upper transformation temperature or when an austentic or P No. 10H material is solution annealed after welding.

On Sat, May 22, 2021 at 9:19 AM Manoj Mumbai <manojacgnr@gmail.com> wrote:
Dear Experts,

The preheat temperature shall not be less than 55 deg. C as per QW-406.1 but  not specified a maximum how much it can be from the temperature noted in PQR as preheat temperature is minimum temperature and interpass temperature is the maximum temperature.
My question , Is there any limitation to increase preheat temperature than mentioned in PQR. suppose PQR temperature is Ambient, say 38 deg. C, can we increase preheat temperature to 204 deg. C.  I have a qualified procedure of P6 material at ambient temperature 38 deg.C now I have to include preheat temperature.

Thanks in advance for your expert opinion.
Manoj.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACgUO5%3DH94mRN3EHOgHBCxM3%2BuEJp3uqYP6qOrOjVbzrD0_bxg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKkEhmUzbSoM%3D%2BA0KrFey8kktejpzZDTGyfx%2BqZNx8fPNFHbmQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...