build‐up of base metal (restoration of base metal thickness):
This is the application of a weld material to a base
metal so as to restore the design thickness and/or structural
integrity. This build‐up may be with a chemistry different
from the base metal chemistry which has been
qualified via a standard butt-welded test coupon. Also,
may be called base metal repair or buildup.


On Mon, May 10, 2021 at 6:46 AM jaimin...@gmail.com <jaiminthejack@gmail.com> wrote:
Dear Gents,

we have situation where client have some component like shaft/Tube Solid  of nickel Grade Material and on the surface they have some material loss.

They want to make grinding>welding>maching to restore the original configuration.

  1. Applicable Code ASME SEC. IX.
  2. Required welding max 5mm.
  3. Shaft Dia varies From 1" to 6"
  • Now as i see we can make WPS/PQR based on QW202.3.
  • But I m confused on selection of Base metal thickness and Grove what we need to suggest.
  • Client don't have metal sheets to make on PQR on that they have only Solid Tubes.

kindly give your value inputs on this regard's.
Thanks & Regards
Jaimin Patel
B.E Mechanical
ASNT NDT L-III(222210)
Email : jaiminthejack@gmail.com 
Skype : jaimin0011
WHATSAPP : +919099018587
 
Failure is simply the opportunity to begin again, this time more intelligently. Henry Ford

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/99a50403-988c-4b59-b32d-e8c24d4c8524n%40googlegroups.com.


--
With Regards

Udaya bahaskar.D

+919676270121

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANii3RM%3DG6GMAYP71ftL5OMzBMVOL%3DwAVDoUOJ0yv%2BUSppfdsA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...