Thank you, dear Ramon, 

Yes, there is a lot, including ASME Sec.II, C. and Grouping in ASME Sec.IX, But, we need a proper reference like you said API 577 etc. 

Looking for other information too, for knowledge. All the best!

Regards, 

Venkat G.

On Thu, Jun 3, 2021 at 7:24 AM Ramon Briceno <bricenori@hotmail.com> wrote:
Dear Venkatachalam,

Please consult the API 577 "Welding Processes, Inspection, and Metallurgy". It has information on electrode table and classification, of course there are many more, from welding technical firms, manufacturers, etc.

Regards, 
Ramon Briceño
Metallurgical Engineer.

Enviado desde mi smartphone Samsung Galaxy.


-------- Mensaje original --------
De: Venkatachalam Govindan <vinisaa@gmail.com>
Fecha: 2021/06/02 8:19 AM (GMT-04:00)
Asunto: [MW:32407] Welding Electrode Selection Table

Dear Respected Professionals, Gday.

We need a welding rod selection table, or suitable comparison table or the proper reference to select the electrode to any particular material if required. Hope our friends will help me. Thank you. All the best. 

Best Regards,
--
Venkatachalam Govindan
QHSE Lead | Auditor | Trainer
(API U Trainer | IRCA Lead Auditor | Exemplar Global MS Specialist |CQI Practitioner)
Mobile +965-97604989

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHOK3OdqswNz6gvYtwT%2BUY%3DckN5MC%2BbqhzOMF-zMSqidvwXL-w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/MN2PR06MB6525D7744E45DE19E2BF2F10AA3D9%40MN2PR06MB6525.namprd06.prod.outlook.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHOK3Oe7Ja5_LjrT6S447YXdpiO7%3DRL1v5wtsohjhmG5z_mSSg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...