Re: [MW:32377] Filler Wire selection

Dear sir,
The pipe and flange will be operated in the same condition, so why did you weld SS316L (pipe) to SS316L (Flange)
I think that is more easy

Vào Th 3, 18 thg 5, 2021 vào lúc 10:16 Rajendra Jadhav <raj04aug@gmail.com> đã viết:
Dear All,

Hope you all are doing well,

I have an query while doing selection of welding filler wire for combination of SS316 L  and Titanium Gr.2 materials welding procedure specification.
Application - Pressure vessel Part {Pipe (SS316L) to Flange (ASTM B862) connection}
Please guide me for the same.

Thank you in advance. 

Best Regards,

Rajendra

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKtLVJwXs7d8TxFte5rYBqGj0inEeOK%3DDE%2Bjv5G4Geujsdd4GA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHTP-OmbcfA0--hzAbJFfHvJ9cKfBzAstPv2rk_Q2qmcVmwEFA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...