Wednesday, April 14, 2021

Re: [MW:32235] PWHT REQUIERMENT FOR PIPING AND PIPELINE

For Pipeline construction please refer to Design Code either ASME B 31.4 or ASME B31.8 as Applicable.

A 333Gr.6 is exempted from PWHT as below.

Inline image

Inline image

Thanks & Regards

J.Gerald Jayakumar




On Wednesday, 14 April, 2021, 08:02:42 am IST, QA/QC <adnanziad49@gmail.com> wrote:


Dear masters 

we want to weld a pipeline api 5l x70 thhikness 28 mm so we want to know the requierement of PWHT CODE API 1104 

AND ALSO FOR A333 GR 6 THICKNESS 45 MM CODE B31.3  . PWHT REQUIERMENT 

CAN ANYONE CLARIFY IT FOR ME 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1123834c-5b79-4fd8-8864-0deaf7c0e3fcn%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...