Re: [MW:32073] Nitrid Precipitation in Duplex SS (ISO 17781 QLll)

Dear Ilkin Hasanov ,

 Acceptance of Nitrid precipitations is depending on if CVN and ASTM G 48 test passed or not .. just to be recorded in the report  


Best Regards ,
Ahmed Osman



On Thursday, March 18, 2021, 06:07:45 a.m. GMT+3, Ilkin Hasanov <ilkinhasanov.91@gmail.com> wrote:


Hi All,

Could you please advise,
If during micro-structural analyse  it were observed Nitrid Precipitates , how need to evaluate test results (mechanical test was done according ISO17781 QL 2)
I want to note that, Specimens were taken for WPQT of Duplex SS, MDT is -25Celsius
PQT coupon dimensions are WT=18mm OD=168.3mm.
Corrosion test results are acceptable ,There was no observed any pittings & Charpy V test results are acceptable (@-46celsius)


Regards, 
Ilkin Hasanov.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADrxeDam%2BqjauoyQHuY274tVCom4GRzoWEr0umXVKN7ScuwO-A%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...