Need separate PQR  as S275 is unassigned material 

On Sat, Mar 6, 2021 at 3:08 PM Vishnu Nandan <nandan.vishnup@gmail.com> wrote:
Hi
I have a qualified WPS for S275JR to S275JR. Can I use the same WPS to weld S275JR to A36.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/51ecf34c-72ac-4780-a050-c0d45b9f41b6n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3OEJ0mDagpRNQwdp8kDUezz%3DRv6_ir81DoFrnHE%3D92GeQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...