[MW:31983] ASME B31.3_2018- Table 331.1.1-PHWT minimumn Holding Time for base material thk-75mm

Dear Experts

Need your guidance in understanding  PWHT minimum  Holding Time base material thk.-65 ~ 75mm

P-No. 1, Group Nos. 1–3
Minimum Holding Time at Temperature for Control Thickness [Note (2)]
-Up to 50 mm (2 in.)-1 h/25 mm (1 hr/in.);15 min min.
-Over 50 mm (2 in.)-2 hr plus 15 min for each additional 25 mm (in.)


Best Regards
Ganesan

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b538da9f-4e78-4b7c-85c3-7679328ed9bdn%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...