Re: [MW:31868] Subject:- Charpy Impact Testing on weld metal

That I know sir, but I want some more information behind this topic why they discarded U notch and For every material they are not using U notch or for which materials U notch is used?

On Thu 17 Dec, 2020, 9:17 AM George Dilintas, <dilintas@gmail.com> wrote:
V notch simulation is more reliable 

Στις Τετ, 16 Δεκ 2020, 06:58 ο χρήστης Shahil Saini <sainishahil98@gmail.com> έγραψε:
Hello everyone, 

My question is, Why ASME BPVC and other standard codes discarded the 'U' notch impact testing?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALfBO_9KBo5H3LU6KOD1xU1LpWHVZwm5SJq4-Z%3DkQDprJTQTrw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40DBBBfmR6sVKsFeL2w_g8SD3Hb1Tv3fu79ZK6TNi_1%3DCA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALfBO__W5fmuqoj4BVvrg4%3DgUJfmFvtUVhG_JHNr5Av14QAAxg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...