Friday, December 11, 2020

Re: [MW:31832] PWHT REQUIRED OR NOT?

Dear Sir,

Construction code ASME SEC VIII Div 1.
Explosive Bonding.

Regards,
Ankit Patel

On Tue 8 Dec, 2020, 2:15 PM 'james gerald' via Materials & Welding, <materials-welding@googlegroups.com> wrote:
Please provide below details.

1. Design Code.
2. Type of cladding like explosive cladding/cold rolling/weld metal overlay(electroslag strip/SAW strip/Laser)

Thanks & Regards

J.Gerald Jayakumar



On Tuesday, 8 December, 2020, 09:09:47 am IST, Prasad Ghanekar <prsgne@gmail.com> wrote:


Refering to SA264
HT is not mandatory for cladding process.
It's suplimentory requirement.

Prasad G.

On Mon, 7 Dec 2020, 16:58 George Dilintas, <dilintas@gmail.com> wrote:
Could you send a sketch of the joint?
You question is not clear

Στις Πέμ, 3 Δεκ 2020 στις 7:34 π.μ., ο/η udaya bhaskar <dusroni@gmail.com> έγραψε:
Hello Mr. Ankith,
Please refer  for your clarification: PART UCL REQUIREMENTS FOR WELDED PRESSURE VESSELS CONSTRUCTED OF MATERIAL WITH CORROSION RESISTANT INTEGRAL CLADDING, WELD METAL OVERLAY CLADDING, OR APPLIED LININGS 

On Wed, 2 Dec 2020, 06:12 Patel Ankit, <aapatel271@gmail.com> wrote:
Dear Expert,

I hope all are well.

My question is In after Tubesheet Bonding PWHT required or Not?

Base Material : SA 516 GR 70. (Thk : 45 mm )
Bonding Material : SA 240 GR 316. (Thk:5mm)

Tubesheet Dia : 3000 mm

( Note : Bonding plate SS 316 : 1 No joint on base material)

Regards,
Ankit Patel
8140255303.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALR-PuwRp0-NoHz6KXB6-4Y3tkTKmaB4pJxtF8HhM8ctpf3EtA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANii3RPebf2pFWS-%2BiPxoJnyobk7eWaxyqNskV1fKD4gJUEqzA%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40BHXNPTU3iqZEqGHpPuxiYd%3DyS-wS_5Tonv6ehAXyTWfw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEi5r3bHEC%2BtYGmUM1Q6%2BNTFAwKboaO9sKyJo7eKj-Hvxj1d%2Bw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/229658807.3500830.1607401509712%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALR-PuwWKNVJBsJ5m6yT5yR%2B6ACVDt-eoCB9-ZXV8js-oPsJQA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...