Tuesday, December 15, 2020

[MW:31846] Polarity

Dear All,

Please Clear me, can we use Polarity DCEN for 6010 electrode welding in piping or pipelines.
If used, explain me how?

  
With Regards

Udaya bahaskar.D

+919676270121

--