Monday, November 23, 2020

Re: [MW:31772] Welding attachements on pipe body

Hi,
What kind of support are u welding?
B31. 8 does have some design requirement for welding attachments mostly the long seam fillet. There is some relation between the hoop stress to the SMYS constraints. 
V do support welding with low hydrogen as our spec calls for it. PQR with fillet fracture and macro ( to check the leg length and fusion) as per api 1104 

On Mon, Nov 23, 2020, 5:47 PM QA/QC <adnanziad49@gmail.com> wrote:
Dear experts 

iHAVE A SCOOP TO WELD SOME ATTACHEMENT ON PIPELINE X52 
There any standard mention about welding attachement on pipe to follow or there also a special WPS AND PQR TO PREPARE 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b91acd31-16e8-417a-b432-1ae6b9063073n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKT-TupoT6gDm9f1FFEEt7%2BfhYv_DV_e2%2BTWLpc%3DQVCMMq6kFg%40mail.gmail.com.

1 comment:

Abdul samadh said...

Any weld to the body of the pipe considered as a part of pressure boundary as such. If u r a material supplier u can follow the same procedure as referred to in material spec., if u r a fabrication contractor u can use the same wps pqr that u use to weld butt joints.u can ask the client what code is mandated in their spec. For pressur part welding on pipe.

[MW:35692]