Saturday, November 7, 2020

Re: [MW:31724] Re: Required pWPS FOR p10H G1 to P1 G1 also P1 G1 to P1 G1

As per Sec 9, no requirement for pWPS, then what to do

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Sat, Nov 7, 2020 at 9:13 AM Bien.ND | weldinginspections.net <bck055@gmail.com> wrote:
Follow specification and refer to ASME IX QW-250. Filling pWPS as guideline here. or you refer to qualified WPS and make it again.

On Tuesday, October 27, 2020 at 9:53:14 AM UTC+7, Fatir Asrar wrote:
Please kindly support me to prepare a pWPS for welding Duplex Stainless Steel to Carbon Steel.
Standard: ASME Sec IX & 31.3
Base Metal: P10H G1 to P1 G1
Thickness: 1.5mm and Above
Dia.: 1" and Above
Process: GTAW
Service: SEA WATER

Kindly upload samples if available. 
Also please let me know the Destructive & NDT tests required for Qualification to obtain supporting PQR.

Also, I need a sample of WPS/PQR for:
Standard: Sex IX & 31.3
Base Metal: P1 G1 to P2 G2
Thickness: 1.5mm & above
Dia.: 1" & above
Process: SMAW

Please kindly do the needful.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/46d1562c-a90d-41df-b00d-812e9c1c4260o%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePO-HuZGMGVEEZ%2B1LP%2BfGVcivDtkinkKYtiSHiuQKAcGQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...