Tuesday, November 3, 2020

Re: [MW:31699] POST HEATING OR dehydrogenation heat treatment

There is no post-heating variable among the essential and not essential variables. Post  -heating is mentioned in QW-409.15 which is related to the electrical characteristics of Resistance Welding
There is Preheat Maintenance (read QW-406.2 to understand the meaning) which is a non-essential variable.
There is PWHT (read QW-407.1 & 407.2). Post heating to remove hydrogen should be treated as PWHT

Στις Σάβ, 24 Οκτ 2020 στις 5:06 μ.μ., ο/η NIKHIL THOMAS JOY <nikhil.thomasjoy@gmail.com> έγραψε:
Dear friends,

Greetings of the day,

I would like to check the post heating details for pipe welded joints for alloy materials.
Please share in which code its available to refer.

My main concern , there is any need to mention post heating in wps or pqr.
if yes, in which code its mention.

Waiting for experts advice.

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/65d036c8-f83f-4f11-8254-1ebbfb28f8d0n%40googlegroups.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40C7juq5LAboAs18H%3DoNbGOxGZy8hhstzV1xPiv1Utj4_w%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...