Saturday, October 31, 2020

Re: [MW:31656] WPS DIAMETER CALCULATION.

Any

On Sat, Oct 31, 2020, 12:25 PM NIKHIL THOMAS JOY <nikhil.thomasjoy@gmail.com> wrote:
Dear Experts,

Greetings of the day.

I have a doubt regarding the WPS preparation. 

I have prepared one PQR of GTAW+SMAW in P22 material of size 6 inch.


But in wps the qualified diameter what I should write as per asme sec 9 , qw-200.


Is this can qualified for all the diameter?
Should i need to write any diameter range in wps.


Even though the thickness range is 5 to 2T.

Experts please advise me.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6c9cd6e7-1d3d-426d-adb7-d361351c767an%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOYh4%2BMGFZif79_2TvbwovMTD_xPfGwMyKbAbgjmBhk%3Dw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...