You might picture in your mind how 'bricks' are laid out or 'concrete blocks'. The Horizontal seams are continuous, however; the 'verticals' are 'offset'. This
is done to prevent a 'crack' starting in one vertical joint from propagating into the next vertical joint. If all the verticals were in one continuous joint, the crack
could propagate from the 1st, into the 2nd, into the 3rd. etc. I hope this helps.

Gene Matsko


On Wednesday, October 21, 2020, 11:51:10 PM CDT, Rajagopal Kannan <rajagopal.kannan@gmail.com> wrote:


Hi,
You Should not have "+" shaped joint.
Thanks and Best Regards,
K.Rajagopal

On Thu, Oct 22, 2020 at 8:42 AM nandakumar pandit <panditns1@gmail.com> wrote:
This means if your shell is in sections, then the longitudinal weldings in all the sections should not be in the same line.

Regards
N. S. Pandit



On Thu, 22 Oct 2020, 10:05 Rajeev Shukla, <gkpshuklaji@gmail.com> wrote:
Sir

I need to under stand the meaning of this line , and which code I should refer for Compressor received welding.

Longitudinal seam in adjacent sections shall not be in same line.

On Saturday, 21 April 2018 at 11:57:35 UTC+5:30 joykol...@gmail.com wrote:
Dear Expert,

Please suggest Dia range.for WPS as per API 1104.

--



Best Regards,

Joydev Dalai
Dy. Manager - QA/QC
Kalpataru Power Transmission ltd.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c23d7c90-1f2b-4a58-ab4d-651cbde1c374n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB7ASHfYfxE5EueVm%3D-RXgMmD%2BY5m9rOPbwAU9q0V9tMRFYhOw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAD3oVpDyqoX%2B%2BoQkahY%2Bn_KotYE%3DaZ5bnAUu4Oj59xQnTPbsMw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...