Re: [MW:31490] Prequalified WPS Essential variables for AWS D1.1 Table3.7 with Table 4.1&4.2

No

On Mon, 21 Sep 2020 at 09:07, QC Engineer <binoypl3@gmail.com> wrote:
Dear Experts,

As per the PWPS essential variables given in Table 3.7 -23 of AWS D1.1,
and comparing it with Table 4.1&4.2,is it permitted to use the Prequalified WPS made for Butt joint welding for FIllet welding also.?


Table 4.1 &4.2 is applicable to Prequalified WPS or not?

Regards



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/70d11f92-f4e5-4719-8604-9131eb30b698o%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BQ29Ohatp-atSuv8A%3D%2BtzAqqjm-4rjbzoypNRz8OSk5h-nhqQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...