Sir,
How much Ph value is required for Hydrotest in Stainless steel piping and equipment.Please advise as per reference of relevant standard & Code.

On Fri 18 Sep, 2020, 5:38 PM Vishwas Keskar, <vvkeskar123@gmail.com> wrote:
use water with Chloride content less than
 25 ppm
use potable water
do water analysis 

On Fri, 18 Sep 2020, 15:38 Manish Kumar, <mkmkr431@gmail.com> wrote:
Dear Sir,
I want to know that which type of water is used for Hydrotest in stainless steel piping and equipment. Please advise as per relevant code and standard.




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHfQ4k7ZV%2B%3DrkXu%3DSdnx2zeGsMf83xjjA%2B4-CLvDzZ1TBuuBfg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3P9%2Bfx%3DaawdsnsTePqFj7W09SMCfy5-tLnkfZ8OS1wHMw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHfQ4k6B4ZuqjvGU7OpupRWFSxN55f3uP4Tw4DssquqyoVUKxw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...