[MW:31500] Re: ASME BPV Sec VIII div1 , UCS-68(b) - PWHT requirements

If a weld joint has a coincident ratio higher then 0,35 then the same need to be PWHT with the following exemptions from PWHT (even if coincident ratio is higher than 0.35):   
Category A and B joints which respect the condition indicated in UCS-68(b)(1) - e.g. 100%RT.
Lightly loaded attachments (<25% stress value) which respect the condition indicated in UCS-68(b)(2)(-a) 
Seal welds (tube to tube sheet)

 It does not exempt from PWHT the category "C" and "D" joints , and fillet welds (except as defined as "lightly loaded attachments" 

On Saturday, 19 September 2020 at 09:01:21 UTC+5:30 MW wrote:
Can you please provide your interpretation for the following requirements of UCS-68(b)
Vessel MDMT - 48 °C , PWHT - not required

In accordance with para UCS-68(b) PWHT is required except for Category A and B joints with 100% RT, lightly loaded attachments and seal welds only.
and it is silent on category C , D welds and other attachments.

Question: does this mean PWHT is required for Category C and D, even though it is exempted for Category A and B welds? then vessel will undergo local PWHT
In my opinion we should not interpret this way and look for only what is code specifies (i.e. if Category A and B or other welds as specified is exempted entire vessel is exempted)  

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/df4bd57b-dfe4-4865-9159-80999d2e474bn%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...