Friday, August 28, 2020

Re: [MW:31363] RE: 31360] Re: As per ASME Sec IX Ed. 2019, ASME Sec VIII, Div-1 and API RP 582

ASME Sec IX Ed. 2019, ASME Sec VIII, Div-1, and API RP 582

Thank you very much for your response.

On Fri, Aug 28, 2020 at 9:15 PM Vinoth Rajendran <rajvinoth1987@gmail.com> wrote:
Hi,

Your WPS will make as per ASME or API???


On Fri, Aug 28, 2020, 18:17 <pgoswami@rogers.com> wrote:

Hi KK,

 

What's the design  code ? ASME Sec VIII , DIV-1 or ASME B-31.3. Looking at the text below, it sounds  Sec VIII, DIV-1 is the design code.

Look at this curve and the exemption clauses for more clarifications. If this curve exempts BM/thickness from impact test , then weld/HAZ should be exempted from impact also.

 

Thanks.

 

 

Pradip Goswami, P.Eng, IWE

Consultant-Welding-Metallurgical Engineering

 

Cell & Whatsapp-905-9793232.

Personal:pgoswami@rogers.com

 

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf Of K K
Sent: August 28, 2020 6:45 AM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:31360] Re: As per ASME Sec IX Ed. 2019, ASME Sec VIII, Div-1 and API RP 582

 

 Dear Experts,  

  
Can I get a response from you?

 

According to  ASME Sec.8, and MDMT is 5°C.

 

Please send me your valuable reply to my doubts.

 

Thanks and Regards

KK

 

 

On Wednesday, August 26, 2020 at 9:47:06 AM UTC+5:30 K K wrote:

Dear Experts,  

 

Impact testing requirements for  Equipment Anchor Chair to top plate/wash welding, base plate, and plug welding.

According to ASME B31.3  above 25mm impact test required.

So for that,  I have restricted to my thickness range 5.00mm to 25.4 mm in WPS.

But Now my requirements for welding Equipment Anchor Chair to top plate/wash welding, base plate, and plug welding.  up to  32.88 mm,

For the 32.88 mm thickness, I have to conduct an impact test or not required impact test 

Process - SMAW.

P No - P1.Gr.No- 1 to P1 Gr,1/2

Thickness range - 5.00 mm to 32.88 mm.

Material - ASTM 516 Gr.60 to ASTM Gr.70

 

As per ASME Sec IX Ed. 2019, ASME Sec VIII, Div-1, and API RP 582according to mentioned code required Impact test or not?

 

Thanks in advance  

 

Regards

KK

 

 

 

 

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/49f11814-bb8f-434c-8da9-9551a4ad71a9n%40googlegroups.com.


Virus-free. www.avg.com

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAuAAAAAAAAABVPzeizzeRJsiPziIE5jXQBAMO2jhD3dRHOtM0AqgC7tuYAAAAAAA4AABAAAACyN7NuThHkQ6frJxXVPdcwAQAAAAA%3D%40rogers.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2Ba0BHbqmnvj7bPyvzHkFS_uf5wEVqXB3yjmTHhWtBfowVGb3w%40mail.gmail.com.


--

KIRAN

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMFjUk4anJKhc8sJTaVM-OONF3vc2sswyzMX%3DQpsQ_OwU6W%3D2Q%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...