Re: [MW:31328] Pre heating as per ASME SEC I / VIII DIV I

As far as designers are concerned they talk about specified thickness.

Sometimes thickness may be  bit more or less then the specified thickness but within the tolerance band. 

On Mon, Aug 17, 2020 at 9:56 AM Vishwas Keskar Welding Manager WELDING <vvkeskar123@gmail.com> wrote:

Specified thickness of the Pipe is 12.7 mm 
Actual thickness measured is 13mm 

Client specified preheating for  12.7 mm (=/>) =75 Deg C

Is preheating is to be decided on specified thickness or  actual thickness?
Any Construction Code back up >


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/23337554-0c50-46b4-911c-5fdac2322672n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPRS9UPQq_OP-K-qST-2Uiwe3jVGgZv_QCxqqzAo5tgue-YM5Q%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...