Re: [MW:30851] ISO 9606 vs EN 287-1

Dear Sir
Kindly read first 3 pages of EN ISO 9606-1. There it is clearly written that  9606-1 superseded the 287-1 although document prepared according to 287-1 is still valid if requirement of 9606-1 comply.
Thanks
Atul Jha

On Thu, May 7, 2020 at 5:36 PM Ilkin Hasanov <ilkinhasanov.91@gmail.com> wrote:
Gents,

Could you please help me to clarify for myself difference of  ISO 9606 vs EN 287-1???


BR,
Ilkin Hasanov 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADrxeDbG5zAG%3DaAXDoiSK5eo%3DXHXFzQi8y4pjyeK4bg9C7uUHA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC1tTUJ5P0S7VaywMzMx%2BnrUM%2BgB43miuvu%2B-GRmgT12K%2BLmrA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...