X-20 is a nasty steel, just ideas about welding welding consumables, methods would not help. If you have mastered the welding methods and techniques for Grade-91 steel, then handling X-20 would be easy, although this steel is always problematic.
I had handled this steel 30+ years ago for a major power plant project. If you're interested , feel to contact me offline or in LinkedIn.
Regards.
Pradip Goswami, P.Eng

pradip.goswami@gmail.com

On Saturday, April 25, 2020 at 2:01:20 AM UTC-4, Waris Ali wrote:
Dear Experts 

X22 CRMOV12-1 +QT2 what is the requirements of mentioned welding and consumable please advised.

Waris Ali 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e1725123-26ca-45dd-9cb1-040cb0db8236%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...