Tuesday, March 3, 2020

Re: [MW:30585] Tack welder qualification ASME Sec IX

The Tack Welder figure DOES NOT EXIST UNDER THE ASME SCHEME, you have to qualify them as Welders.

El mar., 3 mar. 2020 a las 2:32, 'james gerald' via Materials & Welding (<materials-welding@googlegroups.com>) escribió:
Please refer ASME Sec.VIII Div.I snap shot below regarding tack welds.





Thanks & Regards

J.Gerald Jayakumar



On Tuesday, March 3, 2020, 12:44:43 PM GMT+7, Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:


no
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Tue, Mar 3, 2020 at 10:37 AM Chintan <chintan51@gmail.com> wrote:
Kindly advice how to qualify tack welder for u stamp vessel

Is there any exclusive clause available in asme sec ix like aws d1.1 for tack welder qualification

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ba93bbc5-f6a5-4e13-8323-ca2a3b9f44ce%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePd-csF_2hartJVCNj_Ru_SLw0aezixSwd6U_%2B-Jk8CpQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5181949.2489950.1583224251609%40mail.yahoo.com.


--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SSI-TPI

Móvil +52 1 812 352 4606

Skype: jjjimeneza





--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5Zur%2BfVnRpQBYqLiyQ%2BOe%3DsODkd7b5VJzwigU8uapfGWhbNw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...