Re: [MW:30516] Re: Impact Test

70N??

On Wed, 19 Feb 2020 5:35 pm Ramesh, <rameshkannandevaraj@gmail.com> wrote:

I presume there is no specific service requirements and plates are normalized

 

As per Figure UCS-66M of Sec 8 Div.1, The plate material 516 fouls under curve D. the impact testing is exempted up to -48°C .

 

Reg welding, The electrode E7018-1 is guaranteed impact values at -45°C. Refer Table 3 of SFA 5.1.

 

But its better to have impact tested PQRs for company future use. 

Thanks and Regards

Rameshkannan Devaraj

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"



On Wed, Feb 19, 2020 at 3:39 PM prateik tolani <tolaniprateik@gmail.com> wrote:
Dear experts

We have job with MDMT -30 and -36 Deg C
Shell/Dish - SA516 Gr 70N
material will be received in impact tested condition
need to know whether weld impact test is required or not?
thickness is 8-10 mm.
welding electrode 7018-1

On Wed, Feb 19, 2020 at 2:06 PM prateik tolani <tolaniprateik@gmail.com> wrote:
Dear experts

We have job with MDMT -30 and -36 Deg C
Shell/Dish - SA516 Gr 70N
material will be received in impact tested condition
need to know whether weld impact test is required or not?
thickness is 8-10 mm.
welding electrode 7018-1


Thanks 
prateik

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGNY-_AMkqLQr%2BV0KXTtf%3DG%2BX03SpPg8z92ePJqHXO0PJpZctg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMaSVcHs5XyOXpGeyN2r%2B%3D2C6Yej%2BWoRt2AucX%2Bjh_6xN4eTew%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOxFw8YR6iF1yOFoBR%2BHiwSdUL39SFU7%2Bo6pm8mt0jqZw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...