Re: [MW:30507] Welder Qualification in 3G position by 1G PQR

WPS/PQR is Fine. You can proceed with welder qualification in 3G position.

Thanks & Regards

J.Gerald Jayakumar




On Tuesday, February 18, 2020, 06:04:45 PM GMT+7, Brijesh Maurya <brijeshmaurya492@gmail.com> wrote:


Dear all,
Thanks for your valuable advice.
Please find the attached wps & pqr.
Here position for groove is all.
I think i can qualify my welder in 3G position by using this wps/pqr.

On Tue, Feb 18, 2020, 2:31 PM 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
What is the Applicable code.




On Tuesday, February 18, 2020, 02:02:05 PM GMT+7, 'anand gupta' via Materials & Welding <materials-welding@googlegroups.com> wrote:


Need 3G qualification again. 

Regards 
A p gupta 
ThyssenKrupp 


On Mon, 17 Feb 2020 at 9:27, Brijesh Maurya
Dear expert,
please advice can i use 1G qualified PQR for Welder Qualification in 3G upward position? 
Note: No impact requirement.

regards,
Brijesh Maurya

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOBi_ePzg5MZyLqjYhPdQ%3D%2BGCizchu2u18XR%3DMGhg4LUAye4cg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1522244057.3612883.1581989764346%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/110651160.3201064.1582012021854%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOBi_eNTordr5w64NZzKUdUhM88MVyviH24PLxdjiJg9ZTjLPw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...