Re: [MW:30507] Dish end crack during spinning

Dear,

The photograph shows clear slag entrapped inside and on the sides. Polish the specimen to get a clear picture. Check out your voltage, and travel speed.  Those are the areas of improvement.  

In case of any help contact me. 

Regards, 

Charles V Jacob 
Mob: +91 7034331779

On Tue, Feb 18, 2020, 5:46 PM Chintan Raval <chintan51@gmail.com> wrote:
Dear experts 

Kindly find attached photo of dish end

Seam start & Seam end location I found crack during spinning which is approx 30 mm deep 

Material Sa516 gr 70 
Thickness 50 mm
Weld process SMAW + SAW using E7018-1 & EM12K wire 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOdsS42HBY7MKhtCozepSdjribf7bU7smX0sWs_Aok85P%3DLcPQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKpzM4BRf7amAg%3Dj6VmWDEhJW9yQOOgmPz-U9toaOyFGzeZJ%3Dg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...