Tuesday, February 18, 2020

Re: [MW:30501] Welder Qualification in 3G position by 1G PQR

Welder to be qualified based on Approved WPS>

ASME Sec.IX being the code, PQR qualified in 1G position can weld all positions when Impact test is not required.

Amend the WPS to include ALL position or 3G position and carryout Welder Qualification

Thanks & Regards

J.Gerald Jayakumar




On Tuesday, February 18, 2020, 02:02:05 PM GMT+7, 'anand gupta' via Materials & Welding <materials-welding@googlegroups.com> wrote:


Need 3G qualification again. 

Regards 
A p gupta 
ThyssenKrupp 


On Mon, 17 Feb 2020 at 9:27, Brijesh Maurya
<brijeshmaurya492@gmail.com> wrote:
Dear expert,
please advice can i use 1G qualified PQR for Welder Qualification in 3G upward position? 
Note: No impact requirement.

regards,
Brijesh Maurya

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOBi_ePzg5MZyLqjYhPdQ%3D%2BGCizchu2u18XR%3DMGhg4LUAye4cg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1522244057.3612883.1581989764346%40mail.yahoo.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...