Monday, February 17, 2020

Re: [MW:30493] Welder Qualification in 3G position by 1G PQR

One of the main details that should be written in your questions is which of the Codes you are working on,
Ramesh <rameshkannandevaraj@gmail.com>, is correct for ASME SECTION IX, DOESN'T HANDLE EQUAL IN ALL CODES.

El lun., 17 feb. 2020 a las 7:31, harenath jha (<harenathjha@gmail.com>) escribió:
Weld position is not an essential variable for wps 

On Mon, Feb 17, 2020, 09:27 Brijesh Maurya <brijeshmaurya492@gmail.com> wrote:
Dear expert,
please advice can i use 1G qualified PQR for Welder Qualification in 3G upward position? 
Note: No impact requirement.

regards,
Brijesh Maurya

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOBi_ePzg5MZyLqjYhPdQ%3D%2BGCizchu2u18XR%3DMGhg4LUAye4cg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPRS9UOA0ChxH64nDvNjpoqJh3oQq%2BFTTU%3DWR7AiZPmyU0s%2BfA%40mail.gmail.com.


--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SSI-TPI

Móvil +52 1 812 352 4606

Skype: jjjimeneza





--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5ZurL%3Ds_nf-37uaEnMJEHe6KbcPAm%2BW_%2BTDNPr0ZimSR0X9w%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...