Monday, February 17, 2020

[MW:30493] Re: Welder Qualification in 3G position by 1G PQR

As per the ASME SECTION IX-ED-2019,the position is not a essential variable but AWS D1.1 limits position,it depends up on the applicability.


Regards

Nidhin

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/38a6950d-8f08-4d14-892c-f8a6587d626e%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...