Friday, January 17, 2020

Re: [MW:30399] Hardness after PWHT

Designer will decide hardness value for the HAZ and WELDMENT

On Thu, 16 Jan 2020, 11:47 Dharmesh Mistry, <dhamtech@gmail.com> wrote:
Hi,

Para 12.6 (hardness testing - weld procedure qualification and
production) of API RP 582 to be referred.

Regards,
Dharmesh

On Tue, Jan 14, 2020 at 5:28 PM <patelroshankk@gmail.com> wrote:
>
> Dear Experts please explain what hardness of Weld, HAZ, Parents metal is acceptable for F11 & F22 after Post weld Heat treatment.
>
> --
> https://materials-welding.blogspot.com/
> https://www.linkedin.com/groups/122787
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/22949c81-66b3-46b2-bd4a-5a46a78bc6d2%40googlegroups.com.



--

Thanks, & With Best Regards,



Dharmesh MISTRY

+91 9820735814

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMPvC1DBQyCenaL2iK-RSOxaTA48-xXCBh%3DJdbR49%3DXvWHR%3DRA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8mNrdQtcn3-oKDqZJENmSKsoxvuHqS7xV5_dEacNkm1zQ%40mail.gmail.com.

No comments:

[MW:35692]