Other than E309, it seems to be ok. For E309, check the A no. It may be A9 instead of A8. Pl check in Section 9

On Fri, 17 Jan 2020 8:47 am Muhammed Ibrahim PK, <ibratech@gmail.com> wrote:
Gents,

Please help to find the answer for below. Choices are given below. What would be the answer?

A repair organization has a WPS which states it is qualified for P-8 to
P-8 material welded with E308, E308L, E309, E316, electrodes (SMAW
process). The PQR, supporting this WPS, states the weld test coupons were
SA-240 Type 304L material, welded with E308 electrodes. Is the WPS properly
qualified for the base material listed?

A. Yes
B. No
C. Not enough information given
D. Yes, if properly heat treated

Thanks & Regards
Muhammed Ibrahim PK

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALOPgmNviEu9VaoJQjzFC3gz5ci1_AaJty1vnCukLYVpsTimPg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eM6%3D2frntfP9SDc4sTcb-d%3D2Uxrkzc0Ni7bO_%3Dcg3uV%3DA%40mail.gmail.com.

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...