Re: [MW:30378] Hardness after PWHT

After PWHT for F11 & F22 hardness reduced to 110 HB, it is acceptable ?

On Tue, 14 Jan, 2020, 6:19 PM 'Karthik' via Materials & Welding, <materials-welding@googlegroups.com> wrote:
Hi, 
Please refer Section II Part -A SA 182 . It's specified


Sent from Yahoo Mail for iPhone

On Tuesday, January 14, 2020, 6:15 PM, patelroshankk@gmail.com wrote:

Dear Experts please explain what hardness of Weld, HAZ, Parents metal is acceptable for F11 & F22 after Post weld Heat treatment.

--
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/M27c_onWphw/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1766304718.7446033.1579005997404%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHABvdUjmzBfu0v5sQE8ar6tP8enbEjdteVErZHcEyBkaR8LuA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...