Tuesday, January 14, 2020

Re: [MW:30376] Hardness after PWHT

Hi, 
Please refer Section II Part -A SA 182 . It's specified


Sent from Yahoo Mail for iPhone

On Tuesday, January 14, 2020, 6:15 PM, patelroshankk@gmail.com wrote:

Dear Experts please explain what hardness of Weld, HAZ, Parents metal is acceptable for F11 & F22 after Post weld Heat treatment.

--
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/22949c81-66b3-46b2-bd4a-5a46a78bc6d2%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...