Dear Friend,
So they aren't a continuos, regular defecrs & the appearance of defects are various and very superficial .
I bet it is a mechanical cause.
It is a slight variation in the height of the wire against the wall of pipe during welding caused for ocasionaly ,scraps, small particles, rests of flux or other solids that suddenly are in the base of the trolley that translates the pipes making different the above height.
These aren't the typical pock marks caused for a low ratio of recycled flux in SAW manufactured pipes.
I hope it helps
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/41327734-3c54-4191-958d-e2a544f9bc2f%40googlegroups.com.
Subscribe to:
Post Comments (Atom)
[MW:35692]
Dear all Can I do MPI above painting surface for cs tank Regards, Sriram Srinivasan -- https://materials-welding.blog...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment